Nitrogen Characterisation By Xps Photoelectron Spectroscopy Applied To Nitrogen Containing Phosphate Glasses (French)

XPS spectroscopy was adopted to study nitrogen phosphate glasses obtained by nitriding alkaline polyphosphates with ammonia.