New Families Of Glasses Based On Bi203

New families of glasses based on Bi2O3 were found in the systems Bi2O3-Li2O,B203-ZnO-Si20(Na20,K20) and Bi203-ZnO-CaO(SrO,BaO) and their glass forming regions were determined by melting 6g batches. Glass formation in the Bi203-Zn0-Ba0-Li20 quarternary system was also explored.