Morphological Evolution And Weak Interface Development Within Chemical-Vapour-Deposited Zirconia Coating Deposited On Hi-Nicalon Fibre

The phase contents and morphology of a Zr02 fibre coating deposited at 1050 deg C on Hi-Nicalon by chemical vapour deposition were examined as a function of deposition time from 5-120 minutes.

Author
H Li Et Al
Origin
Stevens Inst Technology, Usa
Journal Title
J Am Ceram Soc 85 6 2002 1561-1568
Sector
Glass Fibre
Class
GF 319

Request article (free for British Glass members)

Morphological Evolution And Weak Interface Development Within Chemical-Vapour-Deposited Zirconia Coating Deposited On Hi-Nicalon Fibre
J Am Ceram Soc 85 6 2002 1561-1568
GF 319