Methematical Modeling In The Glass Industry: An Overview Of Status And Needs

This paper presents an overview of mathematical modeling in the field of glass manufacturing. It reviews the principal categories of mathematical models used in the glass industry, examines their current status, and identifies critical needs in the various areas of mathematical modeling.

Author
M K Choudhary And N T Huff
Origin
Owens-Corning Science & Tech Centre, Granville, Usa
Journal Title
Glastech Ber Glass Sci Technol 70 12 1997 363-370