Manufacture Of Optical Glass Blocks Using A Hybrid System Of Ceramic Crucibles And Continuous Moulding (Spanish)

A hybrid system of ceramic crucibles and continuous moulding for the production of 50 tons/year of optical blanks is described. The design of the process for a Pilot plant in Mexico is outlined.