Low-Emissivity Glass Has A Silver Lining

Due to environmental legislation aimed at reducing carbon emissions and energy use, the international building community is striving to achieve net-zero energy carbon neutral buildings. This article details the benefits of triple-silver, solar control, low-emissivity coatings on architectural glass and presents evidence of the environmental qualities through an independent survey.