Light Hollow Glass Makes 1.5 Litre Bottle Attractive (German)

1 litre disposable bottles coated with PE dispersions and weighing only 260g are being manufactured in West Germany. Returnable glass bottles for carbonated beverages weigh only 700g and a 1.5 litre lightweight bottle priced at 28-36 Pfennigs have also been introduced.

Author
G Wirsig
Origin
Unknown
Journal Title
Informationsdienst Verpack No. 1 Jan 1990 3
Sector
Container glass
Class
C 309

Request article (free for British Glass members)

Light Hollow Glass Makes 1.5 Litre Bottle Attractive (German)
Informationsdienst Verpack No. 1 Jan 1990 3
C 309