Libbey Glass Adopts Successful Approach To Furnace Inspection

US-based PaneraTech Inc has introduced a revised standard in furnace health monitoring for the glass industry, with the ability to measure refractory thickness and identify any glass penetration through furnace walls. However, the most significant benefits to customers are realised over the course of time, as regular furnace monitoring leads to better informed decision-making.