Li2O.2Sio2 Sol-Gel Glass

An explanation of the tendency of sol-gel glasses containing network modifiers to devitrify is proposed.

Author
F Branda Et Al
Origin
Unknown
Journal Title
J Mater Sci Lett 1987 6 2 203-206
Sector
Special Glass
Class
S 56

Request article (free for British Glass members)

Li2O.2Sio2 Sol-Gel Glass
J Mater Sci Lett 1987 6 2 203-206
S 56