Leerco To Deliver New Decorating Lehr

Leerco Engineering has won an order from Stolzle Flaconnage for a 3.66m wide electric decorating lehr for the glassmaker's plant at Knottingley. The lehr is due to be commissioned early 2007 and will fire prestige spirits bottles. It will be fed from a three colour automatic printing machine. This will offer Stolzle Flaconnage more than double its current capacity on the line.