Leached Antireflection Surfaces Part 4. Proposed Model For The Neutral Solution Process

A mechanism for the leaching process based on the effects of Al3+ adsorption from solution onto the glass surface is proposed.

Author
L M Cook
Origin
Schott Technologies, Inc
Journal Title
Glastech Ber 1987 60 11 368-375