Latest Systems Enhance Cullet Quality

Contamination with even the smallest inclusions of ceramic, stone, porcelain or off-colours can cause significant deficiencies in cullet quality. In this paper a number of systems designed to ensure that the quality of cullet is as high as possible are examined.

Author
P Mayer
Origin
S & S Metallsuchgerate Gmbh, Germany
Journal Title
Glass 76 10 1999 334
Sector
Container glass
Class
C 1461

Request article (free for British Glass members)