Laser Cutting Decorative Glass, Ceramic Tile

Accurate cutting of intricate and small-sized shapes in nonhomogenous ceramics such as decorative tile and glass, necessitates a high degree of skill and expertise on the part of the artisan.

Author
I Black
Origin
Heriot-Watt University, Scotland
Journal Title
Am Ceram Soc Bull 77 9 1998 53-57
Sector
Domestic glass
Class
D 362