Kinetics Of Crystallisation Of Zr20Ti20Cu60 Amorphous Alloy Using Modulated Differential Scanning Calorimetry

Ti-Cu-Zr system forms glasses in a wide composition range and also shows a large undercooling. This makes them suitable candidates for bulk glass formation using copper mould casting. In this work, the kinetics of crystallisation of Zr20Ti20Cu60 amorphous alloy has been investigated from room temperature to 773K by DSC.