Kinetics Of Alkali Silicate And Aluminosilicate Glass Reactions In Alkali Chloride Solutions: Influence Of Surface Charge

Initial rates of alkali ion exchange from sodium trisilicate, potassium trisilicate, lithium disilicate, and several sodium aluminosilicate glasses were measured as a function of electrolyte concentration and pH (concentration scale) using pH-stat methods.