Ir Spectroscopy Of Glasses Of The System 0.3Lif.0.7Napo3-Mfx(M=Mg,Ca,Al)

The glass-formation region in systems with CaF2 ({15mol%) is much smaller than systems with MgF2 ({41mol%) and Al ({43% mol). Density, viscosity, and electrical conductivity reflect the macrostructure properties of the glass and rearrangement of the structure. This rearrangement of the structure is related to the breakdown of the metaphosphate chains.