Introducing The New Sd6000 Printing Machine For Uv-Curable Organic Inks

Glass is emerging as a universal packaging mediam with the ability to give products packaged in glass a unique, durable and value-added appearance through the use of creative and ingenious decorating techniques. This paper looks at the new SD6000 printing machine for UV-curable organic inks.