Influence Of Several Metal Ions On The Gelation Activation Energy Of Silicon Tetraethoxide

The effects of nine metal cations on silica gel formation have been investigated by studying the hydrolysis and polycondensation of silicon tetraethoxide in the presence of metal nitrates.