Influence Of Processing Conditions On The Viscosity Of Silicate Glass (In Italian)

This paper examines various silicate glass systems, and demonstrates by means of viscosity measurements that different processing temperatures may affect the microstructure of the glass.

Author
G Bonetti
Origin
Unknown
Journal Title
Rivista Della Staz Sper Del Vetro 22 4 1992 179-188
Sector
Special Glass
Class
S 690

Request article (free for British Glass members)

Influence Of Processing Conditions On The Viscosity Of Silicate Glass (In Italian)
Rivista Della Staz Sper Del Vetro 22 4 1992 179-188
S 690