The Influence Of Oxide Additions On The Oxidation States Of Polyvalent Dopants In Zblan Glasses

The effect of Zr02 additions on the oxidation states of the polyvalent elements Fe, Cu, Cr, In and Eu in ZBLAN glasses have been investigated. The oxidation states of the various dopants were examined by optical absorption spectroscopy of the glasses and the oxygen content was determined using the LECO combustion method.

Author
S Aasland & S Julsrud
Origin
University Of Trondheim, Norway
Journal Title
Phys Chem Glasses 37 6 1996 239-247
Sector
Special Glass
Class
S 1105

Request article (free for British Glass members)

The Influence Of Oxide Additions On The Oxidation States Of Polyvalent Dopants In Zblan Glasses
Phys Chem Glasses 37 6 1996 239-247
S 1105