Influence Of Modifier Cations On The Radiation-Induced Effects Of Metaphosphate Glasses

The influence of different modifying cations on the radiation-induced defect generation in meta phosphate glasses was studied by optical absorption and electron paramagnetic resonance spectroscopy.