Increasing The Wear-Resistance Of Mould Sets For Shaping Glass Containers

Causes of disruption of parts of mould sets for pressing and blowing machines are investigated. Recommendations for their reinforcement are presented.

Author
V A Timoschchenko
Origin
Elia-Vit Scientific & Engineering Centre, Russia
Journal Title
Glass & Ceramics 53 1-2 1996 61-62
Sector
Container glass
Class
C 1297