Hydrogen Reactivity Of Barium Galliosilicate And Related Glasses

This paper reports the results of an investigation of the use of hydrogen reaction with the glass structure to probe the defect structure of the glass.

Author
C M Shaw, J E Shelby
Origin
Alfred University, Usa
Journal Title
Physics And Chem Of Glasses 34 3 1993 88-94
Sector
Special Glass
Class
S 725