How To Increase The Life-Span Of The Pot

The Centre for Development of Glass Industry conducted a scientific study on the factors that go into the making of a good pot. It created improved prototypes and conducted field trials in Firozabad, proving that 60 days' pot life - as against the present 15-day average - is within reach.

Author
R N Bhargava
Origin
Unknown
Journal Title
Kanch 9 2 2001 6-8
Sector
Domestic glass
Class
D 571