High Resolution Solid State Nuclear Magnetic Resonance Of The Ternary Silicate Glass Sio2-Tio2-Zro2 Prepared By The Sol-Gel Method

Magic angle spinning nuclear magmetic resonance has been used to study the structural evolution of a three-alkoxide gel system towards the ternary 65SiO2, 20TiO2, 15ZrO2 glass, which is not accessible by conventional melting.

Author
Ch Wies Et Al
Origin
Universitat Munster, Technische Universitat Clausthal
Journal Title
Phys Chem Glasses 1990 31 4 138-143
Sector
Special Glass
Class
S 423

Request article (free for British Glass members)

High Resolution Solid State Nuclear Magnetic Resonance Of The Ternary Silicate Glass Sio2-Tio2-Zro2 Prepared By The Sol-Gel Method
Phys Chem Glasses 1990 31 4 138-143
S 423