Heating And Blackening Of Lehr Conveyor Belts

In this paper the author describes a new method to optimise the heating and blackening of the lehr belt that glassmakers need for optimum products.

Author
F Corner
Origin
Minasgas, Brazil
Journal Title
Glass Int March/April 2002 28