Heat Transfer Modelling Of The Parison Forming In Glass Manufacturing

Parison formation in a narrow neck press and blow process for glass container forming is studied. Heat transfer in the plunger, glass and blank mould during parison formation is analysed by a numerical model. A finite difference formulation is used for the heat transfer calculations.