Halide Glasses: A New Laser Matrix (French)

A survey of laser operations reported for heavy-metal fluoride glasses is presented. Some spectroscopic mechanisms are proposed to intensify the radiative transitions of rare-earth ions.

Author
J L Adam, P Le Gall, J Lucas
Origin
University Of Rennes
Journal Title
Rivista Della Staz Sper Vetro 1989 1 97-102