Glass Viscosity Calculation Based On A Global Statistical Modelling Approach

A viscosity model for predicting the complete viscosity curve of glass was developed using a global statistical approach & more than 2200 composition- viscosity data for silicate glasses collected from over 50 years of scientific literature, including soda-lime-silica container & float glasses, TV panel glasses, borosilicate fibre wool & E type glasses, low expansion borosilicate glasses, glasses for nuclear waste vitrification, lead crystal glasses, binary alkali silicates, & various other compositions. It is shown that, within a measurement series from a specific laboratory, the reported viscosity values are commonly overestimated at higher temperatures due to evaporation losses during the measurement & glass preparation; this data presented by Lakatos et al ( Glass Technology 1972)

Author
A Fluegel
Origin
Pacific Northwest National Laboratory,Washington, Usa
Journal Title
Glass Technology February 2007 Volume 48 1 13-30
Sector
Special Glass
Class
S 3303

Request article (free for British Glass members)

Glass Viscosity Calculation Based On A Global Statistical Modelling Approach
Glass Technology February 2007 Volume 48 1 13-30
S 3303
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.