Glass Strengthening With A Femtosecond Fibre Laser

Laser-matter interactions and mechanisms for future formation in transparent materials is a trend research area. According to the author of this paper, by the use of a femtosecond fibre laser, up to 50% increases in mechanical strength have been obtained by setting the appropriate fibre laser parameters.

Author
D Ariburnu Et Al
Origin
Sisecam, Turkey
Journal Title
Glass Worldwide May-June 2016 112-114