Glass With Special Effects

This article discusses advances in coating technology and in particular how an extremely thin film of silver on window glass reflects heat radiation but allows visible light to pass through, thereby improving the energy efficiency of buildings and vehicles.

Author
A Herzog
Origin
Buhler Alzenau, Germany
Journal Title
Glass Worldwide Sept-Oct/2016 110
Sector
Flat glass
Class
F 3898