Glass Panacea: A User-Friendly Free Software Tool For The Formulation Of Glasses, Glass-Ceramics, And Ceramics

Determining which chemicals from the periodic table, and how much to use, is a time-consuming task when preparing a batch formulation. This article describes a newly developed software tool which eases the selection of chemicals and improves the accuracy of calculations for formulations of glasses, glass-ceramics, and ceramics. The tool can be downloaded from: www.certev.ufscar.br/research-1/glasspanacea-glass-and-ceramic-formulati...

Author
R L Siqueira Et Al
Origin
Unknown
Journal Title
Am Ceram Soc Bull 96 1 2017 48-49
Sector
Special Glass
Class
S 4343

Request article (free for British Glass members)

Glass Panacea: A User-Friendly Free Software Tool For The Formulation Of Glasses, Glass-Ceramics, And Ceramics
Am Ceram Soc Bull 96 1 2017 48-49
S 4343
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.