Glass Keeps Batteries Healthy

The better lithium-ion batteries or super-capacitors work, the more electric vehicles will populate our roads. A new building block can help: Schott GTAS battery lids with hermetic glass-aluminium seals increase the safety and service life of storage cells, and pave the way for a more compact design, higher capacity and longer lifetime.

Author
Un-named
Origin
Unknown
Journal Title
Schott Solutions 1/2019 26-29
Sector
Special Glass
Class
S 4547

Request article (free for British Glass members)

Glass Keeps Batteries Healthy
Schott Solutions 1/2019 26-29
S 4547
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =