Glass Decorating Options

This paper looks at the various methods used to decorate glass containers. Direct screening, transfer technology, decal application technology and other options are examined.

Author
A Bopp
Origin
Soc Glass & Ceramic Decorators, Usa
Journal Title
Int Glass Review 3/2001 83-85
Sector
Container glass
Class
C 1847

Request article (free for British Glass members)

Glass Decorating Options
Int Glass Review 3/2001 83-85
C 1847