Glass Decorating Inks Require Clear Thinking

In this article the author describes the shift towards organic UV inks for the decoration and labelling of glass products, explaining their value to glassmakers in terms of cost-effectiveness, ease of use and freedom of design; qualities that are receiving increased attention in light of recent health and safety legislation.

Author
R Mcmillan
Origin
Sun Chemical, Uk
Journal Title
Glass International November 2010 13-14
Sector
Container glass
Class
C 4283