Glass Blocks That Conserve Energy

Energy saving glass blocks are the ideal building material for creating environmentally-friendly buildings without sacrificing design. The results of exclusive technology patented by Seves Glassblock, these innovative glass blocks significantly improve the heat dispersion of the glass by lowering its thermal transmittance to U=1.5 W/m2 K (from U=2.8W/m2 K). Energy Saving glass blocks make it possible to maintain the ideal temperature inside, no matter what the weather is like outside, without consuming additional energy or resources. These innovative glass blocks are available in the standard 19x19x8 neutral format, in the smooth or wavy glass design with transparent or satin finishing (on one, or both sides).

Author
Un-named
Origin
Unknown
Journal Title
Gmpa 4/2014 11
Sector
Flat glass
Class
F 3596

Request article (free for British Glass members)

Glass Blocks That Conserve Energy
Gmpa 4/2014 11
F 3596
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.