General Insight Into Vessel Glass Conservation And Its Ethics

A general insight is given into vessel glass conservation and the different ethical approaches which are taken between archaeological and historical glass. How the age of the glass, its inherent stability, and surrounding environment will influence not only preservation but also the approach which is taken to conservation.