Gamma Irradiation And Heat Treatment Of Ion Exchanged Silver Containing Glasses

A study of the effects of either irradiation alone or combined with thermal treatment on the colour and spectral absorption of Ag containing soda-lime-silica glasses was conducted to explore the effects that irradiation may have on the mechanism of Ag staining.