Furnace Crown Successfully Repaired At Indian Plant

In mid-1999, Lubisol Engineering Co carried out hot repair work on a furnace in India using its newly developed hermetic sealing patch. The most recent inspection of the repair earlier this year revealed that the crown is now in a stable condition.

Author
Prof S Lutskanov & R Singh
Origin
Lubisol Eng, Bulgaria & Vitrum Glass, India
Journal Title
Glass Int 23 3 May-June 2000 12-13
Sector
Container glass
Class
C 1556