Ftir, Epr & X-Ray Investigation Of Mixed Valence Molybdenum Phospahte A20-(Moo3)2-P205(A=Li,Na) Glasses

FTIR transmittance spectra and EPR investigation of three series of glass in the system A20-(MoO3)2-P205 (A=Li, Na) have been studied.