Fracture Analysis Of Glass Containers (Portuguese)

The basic principles of fracture analysis are reviewed briefly with diagrams of typical types of fracture

Author
M Untama
Origin
Vidrios Industriales S/A
Journal Title
Vidro November/December 1988 9-11