Forming Of Glass Tubing (Italian)

The Danner process for forming glass tubing is described. Possible developments, particularly with respect to control, are discussed briefly.

Author
S Miglioli
Origin
Olivotto Spa
Journal Title
Vetro Informazione November-December 1987 42 28-29, 32-36
Sector
Special Glass
Class
S 70