Formation Of B-Silicon Nitride Crystals From (Si-Al-Mg,Y)(O,N) Liquid: Ii, Population Dynamics And Coarsening Kinetics

Precipitation, growth, and coarsening of Si3N4 crystals in liquids at 1680 deg C have been studied.