The Fluorozirconate Glasses

The state of the art with regard to the structure of fluorozirconate glasses is reviewed with particular reference to results of Raman spectroscopy and X-ray diffraction studies.

Author
E Czerwosz
Origin
R And D Center Of Vacuum Electronics, Warsaw
Journal Title
Bol Soc Esp Ceram Vidr 1990 29 5 353-356
Sector
Special Glass
Class
S 477