Fluorescence Spectral And Energy Transfer Studies Of Sm3+:Pr3+ System In Chlorophosphate Glass

Optical absorption and emission spectral studies of Sm3+Pr3+ co doped system in chlorophosphate glass system is reported with special emphasis on the non radiative energy transfer between these ions.