Flow In Glass-Melting Furnaces

Time lapse photography of the interior of glass melting furnaces has been shown to be a useful technique for evaluating furnace performance. The results indicate that the end fired furnace is at a disadvantage compared with a cross fired furnace. The importance of temperature distribution, a well-developed thermal and properly controlled charging patterns were emphasised.