[Float Glass Analysis] China - Empty Chairs And Empty Tables - Where Has All The Float Glass Gone?

China is the world's number 1 producer of float glass, accounting for 55% of the world's production capacity. As of June 2016, there were 296 float lines available in China. Of this 226 lines were in operation with a total capacity of 150,179/tpd. Those who have been importing float glass from China for the last few months will have noticed a phenomenon of unusually strong demand from China's domestic market. This article takes a closer look at the dramatic changes China's float glass industry.

Author
J Sim
Origin
Unknown
Journal Title
Asian Glass December 2016 42-44
Sector
Flat glass
Class
F 3933

Request article (free for British Glass members)

[Float Glass Analysis] China - Empty Chairs And Empty Tables - Where Has All The Float Glass Gone?
Asian Glass December 2016 42-44
F 3933
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.