Fabrication Of Micro Structures Composed Of Metallic Glasses Dispersed Oxide Glasses By Using Micro Stereolithography

Magnetophtonic crystals with periodic arranged magnetic materials can reflect the terahertz waves through Bragg diffraction. The micrometer order magnetophotonic crystals were fabricated by stereolithographic methods.

Author
M Nakano Et Al
Origin
Osaka University, Japan
Journal Title
Ceramic Transactions Vol 231 2012 187-191 (Proc 9Th Int Conf On Advances In Fusion (Afpg9), Australia
Sector
Special Glass
Class
S 4423

Request article (free for British Glass members)

Fabrication Of Micro Structures Composed Of Metallic Glasses Dispersed Oxide Glasses By Using Micro Stereolithography
Ceramic Transactions Vol 231 2012 187-191 (Proc 9Th Int Conf On Advances In Fusion (Afpg9), Australia
S 4423
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.