Explanation Of Flow On Flat Glass Tanks

In most flow models the migration rate of definite vol elements is described; this is not sufficient for process analysis because the progression rate of the max effect is not known. This rate is different in each circulation loop and a correlation method is presented which determines the rate in each loop.

Author
W.D. Hamisch
Origin
Unknown
Journal Title
Silikattechnik, 25 [4] 126-27 (1974)