Experimental Research And Analysis On The Viscosity Of Basalt Melt And Basalt Additives At High Temperatures

The viscosity of basalt melt and its dependence on temperature and chemical composition are important for studying the application of basalt as fibre, ceramic materials or glass. I this paper the viscosities of Wanquan basalt melt and other samples, which are composed by introducing defined quantities of additives respectively, and the relationships between the viscosities and basalt melt's chemical compositions are experimentally studied and analysed.

Author
S Deku Et Al
Origin
Hebei University, China
Journal Title
Glass Technology 42 4/5 2001 134-138
Sector
Special Glass
Class
S 2318

Request article (free for British Glass members)

Experimental Research And Analysis On The Viscosity Of Basalt Melt And Basalt Additives At High Temperatures
Glass Technology 42 4/5 2001 134-138
S 2318
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.